Top

Metal Hardness Conversion Chart

Resources / Hardness conversion chart

Convert between Rockwell C, Rockwell B, Brinell, and Vickers hardness for carbon and alloy steels, with approximate tensile strength. Enter a value below or pick any row from the full chart.

Hardness converter

Convert from
HRC

Rockwell C values from 20 to 68 HRC.

Equivalent values

Rockwell C
Rockwell B
Brinell
Vickers
Tensile strength
Tensile strength

Where it sits on the hardness scale

Typical hardness for common steels after heat treatment. Actual results depend on the specification, section size, and tempering temperature.

Soft to hard

Full hardness conversion chart

Approximate equivalents for non-austenitic steels, based on ASTM E140 conversion tables. Select any row to load it into the converter.

Rockwell CHRC Rockwell BHRB BrinellHB, 3000 kgf VickersHV Tensileksi, approx. TensileMPa, approx.

Conversion values are approximate and provided for reference only.

Reading the scales

Rockwell C (HRC)

Diamond cone indenter under a 150 kgf load. The standard callout for hardened steel from about 20 HRC up.

Rockwell B (HRB)

1/16″ steel ball under 100 kgf. Used for softer annealed or normalized steel, below the useful range of Rockwell C.

Brinell (HB)

10 mm ball under 3000 kgf. The large indent averages out coarse grain, so it is common on forgings and castings.

Vickers (HV)

Diamond pyramid indenter. One continuous scale from soft to fully hardened steel, and the usual choice for thin sections and case depth surveys.

Tensile strength

An estimate of ultimate tensile strength for carbon and alloy steel. Use it for early design checks, not for certification.

Hardness conversion questions

How accurate are hardness conversions?

Conversions between scales are empirical approximations, not exact equations. They are dependable for non-austenitic carbon and alloy steels. For acceptance testing, always test in the scale your specification calls for rather than converting.

When should I use Rockwell B instead of Rockwell C?

Use Rockwell C for hardened steel at roughly 20 HRC and above. Below 20 HRC the diamond indenter loses sensitivity, so softer annealed or normalized steels are tested on Rockwell B.

Can you estimate tensile strength from hardness?

For carbon and alloy steels, hardness gives a useful estimate of ultimate tensile strength. The relationship does not hold well for stainless, non-ferrous, or very hard brittle steels, and it never replaces a tensile test.

Why does the Brinell column stop around 650 HB?

Brinell testing uses a ball indenter that starts to deform on very hard steel. Above roughly 650 HBW, labs switch to Rockwell C or Vickers.

Need parts held to a hardness callout?

A conversion chart gets you close. Hitting the number on your print is our job. Rex Heat Treat hardens, tempers, and case hardens to your specified HRC, HRB, or HV range, with results verified in our on-site metallurgical lab. NADCAP, ITAR, ISO 9001, and CMMC 2.0 Level 2 certified.

Request a Quote